@artistpavel: did you use primer as a undercoat? I use flat Krylon too but I primed my surfaces first (2 coats). Sticks pretty well. If you can't find self etching primer, Stix or Zinsser Bulleseye works well for primer too. Also remember paint takes time to cure. If the paint hasn't had time to cure it can get nicked or scratched easily. I leave the newly painted case alone to cure for 2 weeks before I start putting anything in it. Actually ,1 week should be enough but the longer the better.

Last edited by morphy; July 30, 2009 at 08:58 PM.